Powder instructions for Poor film build – Too Thin

Poor Film Build, Too Thin:

  1. Marginalized ground

Recheck electrical continuity for the conveyer

Equipment suppliers have a resistance ohms limit for the line. Confirm you are below that limit high resistance gives the gun a varying voltage from beginning to end of spray

Poor Ground shows up often as a pattern of poorly coated area on parts. Without proper ground parts build up charge so the effective charge of the gun is reduced.

  1. Use clean hooks with sharp contact to the part

Scrape clean as needed

High resistance

  1. No unused hooks through the spray booth

Coating Unused Hooks eliminates the ground by insulating the contact points



This post first appeared on Forrest Technical Coating Experts, please read the originial post: here

Share the post

Powder instructions for Poor film build – Too Thin

×

Subscribe to Forrest Technical Coating Experts

Get updates delivered right to your inbox!

Thank you for your subscription

×